Product details
Model Number: high speed steel-01-42
Key Specifications/Special Features:
M42 high speed steelApplications:High-carbon, high-speed steel grade based on Mo, with high resistance to wear, red hardness and toughness. This steel grade displays good grind ability as a result of its low V content. Tools severe mechanical wear, e.g. in cases of small cross-section cuts and high cutting speeds. Particularly suitable for die-sinking cutters and one-lip cutters, and for tool bits in automatic lathes. Also suitable for non-cutting applications, e.g. cold extrusion rams, and for tools for machining aircraft materials, such as titanium alloys, etc.Steel Grade:C:1.05 - 1.15Si:0.15 -0.50Mn:0.15 - 0,40P:<=0,030
S: <=0,030
Cr:3.50 - 4.25
Mo:9.00 - 10.00
V: 0.95 - 1.35
W: 1.15 - 1.85
Co:7.75 - 8.75
Size available:
Anneal temperature: 860-880
Relief annealing temperature: 720-760
Hardening temperature: 1160-1190
Hardening medium: salt bath under 600,aslo use oil cooling or air cooling
Normal temper temperature: 540-560
RC Rockwell hardness after hardening and temper: 66-68
Characteristic: High performance tungsten-molybdenum high speed steel, excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness
High speed steel got hardness method:
- Round and square bar: 2-300mm
- Flat: thickness: 0.6-250, width: 30-810mm
Relief annealing temperature: 720-760
Hardening temperature: 1160-1190
Hardening medium: salt bath under 600,aslo use oil cooling or air cooling
Normal temper temperature: 540-560
RC Rockwell hardness after hardening and temper: 66-68
Characteristic: High performance tungsten-molybdenum high speed steel, excellent performance of hardness, red hardness, thermoplasticity, machinability. Only weak in toughness
High speed steel got hardness method:
1. Salt bath hardening or vacuum hardening
2. The temperature 1180-1200°C, if need high hardness add 10°C 3. in the temperature 560°C, tempering more than 3 times. The most important: control hardening temperature and time.
2. The temperature 1180-1200°C, if need high hardness add 10°C 3. in the temperature 560°C, tempering more than 3 times. The most important: control hardening temperature and time.
Shipping Information:
- FOB Port: China (Mainland)
- Lead Time: 5 - 45 days
Main Export Markets:
- Asia
- Australasia
- Central/South America
- Eastern Europe
- Mid East/Africa
- North America